MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
NuSil CF2-2186 Silicone Two Part Sealing & Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: General Purpose: Two Part Sealing & Adhesive

Comments: Medium Viscosity, All Purpose Potting & Encapsulant

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Viscosity 18000 cPB
 38000 cPA
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20
Tensile Strength at Break 6.20 MPa
Elongation at Break 600 %
Tear Strength 70.0 pli
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 500 V/mil
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Temperature 150 °C
Working Life 2.00 hour
 
Descriptive Properties
ColorTranslucent
Mix Ratio10:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil R21-2615 Silicone Two Part Sealing & Adhesive
Wacker Lumisil® LR 7601/80 Liquid Silicone Rubber
Dow 3-4170 DIELECTRIC GEL KIT
Chosun Refractories SFC-70 SiC Castable
Chosun Refractories SCX-70 I Special SiC Castable

PNUSIL032 / 141756

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.