MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zotefoams Plastazote® LD45FR Low Density Polyethylene Foam, Flame Retardant
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

Compliant with EC food contact and US FDA regulations.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0390 - 0.0490 g/cc0.00141 - 0.00177 lb/in³sheet density
 0.0450 g/cc0.00163 lb/in³Nominal skin/skin; BS ISO 7214 1998
Cell Length 0.400 mm0.0157 inTypical Diameter
 0.250 - 0.600 mm0.00984 - 0.0236 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 606010 mm cell/cell thickness; ISO 868 1985
Tensile Strength 0.435 MPa63.1 psiISO 7214 1998
Elongation at Break 180 %180 %
Compressive Yield Strength  0.0690 MPa
@Strain 10 %
10.0 psi
@Strain 10 %
BS ISO 7214 1998
 0.0860 MPa
@Strain 25 %
12.5 psi
@Strain 25 %
BS ISO 7214 1998
 0.121 MPa
@Strain 40 %
17.5 psi
@Strain 40 %
BS ISO 7214 1998
 0.159 MPa
@Strain 50 %
23.1 psi
@Strain 50 %
BS ISO 7214 1998
Tear Strength 1.20 kN/m6.85 pliBS EN ISO 8067 1995
Compression Set  2.5 %
@Time 79200 sec,
Strain 25 %
2.5 %
@Time 22.0 hour,
Strain 25 %
24 hr recovery; BS ISO 7214 1998
 8.5 %
@Time 79200 sec,
Strain 25 %
8.5 %
@Time 22.0 hour,
Strain 25 %
0.5 hr recovery; BS ISO 7214 1998
 11 %
@Time 79200 sec,
Strain 50 %
11 %
@Time 22.0 hour,
Strain 50 %
24 hr recovery; BS ISO 7214 1998
 20 %
@Time 79200 sec,
Strain 50 %
20 %
@Time 22.0 hour,
Strain 50 %
0.5 hr recovery; BS ISO 7214 1998
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0430 W/m-K0.298 BTU-in/hr-ft²-°Fmean temp of 10°C; ISO 8302 1991
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
 
Descriptive Properties
FlammabilityAutomotive: FMVSS.302 burn ratePass: 2 mm and thicker
 Aviation: CAA8/2-2.2bComplies
 Aviation: FAR-25.853 F 1a. 1iiComplies
 Aviation: JAR-25.853 F 1a. 1iiComplies
 Construction: DIN4102 pt14-B1Pass: 6 to 20 mm thick
 Construction: UL94 HF1+HF2Pass: 3 to 13 mm thick
 Horizontal Burn Rate: ISO 7214 1998Extinguishes and melts from flame

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech Silica Aerogel
ERG Aerospace Reticulated Vitreous Carbon (RVC)
BASF Neopolen® 1710 40 mm Expanded Polyethylene
Zotefoams Plastazote® MP34 Metallocene Polyethylene Foam
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam

PZOTEF920 / 150676

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.