MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polimix S5008 Polyester Sheet Moulding Compound
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: SMC (Sheet Moulding Compound) is a reinforced composite material that consists of a mixture of: thermosetting resins; 25mm glass fiber; Fillers; additional components

Application of this grade: This compound is mainly compression molded. The ability to use reinforcing fibers up to 50 mm allows for high mechanical properties.

Production process: It is produced by mixing polyester resin and the main additives, obtaining a paste with a honey-like consistency, which is pumped into a coating machine equipped with a cutter that, synchronized with the dosing of the paste, adds the reinforcing fiber in a predetermined and constant quantity. A support film ensures that the two layers of dough can be joined to the fiber coming from the cutter, thus creating a sandwich structure with two layers of dough on the outside and the fiber in the middle. The next operation, which is carried out in-line, is the compression of the resulting mattress by means of cylinders and metal nets in order to facilitate the best impregnation between the various components. The SMC is then welded in boxes or wrapped in rolls, the packages are then placed in the curing chamber. After about 24 hours, through the reaction with the thickener the paste becomes solid and allows easy removal of the backing film. SMC formulations are customized according to the customer’s needs, the type of customer’s needs, the type of presses and the complexity of the moulds.

Application of this grade: Electrical Cabinets

Information provided by Polmix SPA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 - 1.80 g/ccISO 1183
Filler Content 20.0 - 27.0 %Glass Fiber; ISO 1172
Water Absorption <= 0.200 %ISO 62
Linear Mold Shrinkage 0.000500 - 0.00100 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 140 - 160 MPaUNI EN ISO 178
Flexural Modulus >= 9.00 GPaUNI EN ISO 178
Charpy Impact, Notched >= 60.0 kJ/m²UNI EN ISO 179
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air >= 200 °CHDT; ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLM917 / 322949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.