MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes:
  • Industrial pallet wrap stretch film applications
  • Premium film packaging applications
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a
TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, designed for cast stretch film applications such as industrial pallet wrap. Films containing HSE-7002 offer outstanding puncture, toughness and load holding properties.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9178 g/ccASTM D792
Thickness 0.800 mil
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1538 psiASTM D882
Film Tensile Strength at Yield, TD 1638 psiASTM D882
Film Elongation at Break, MD 481 %ASTM D882
Film Elongation at Break, TD 891 %ASTM D882
Elongation, Ultimate 295 %on-pallet testing; Highlight Industries Method
Secant Modulus, MD 0.1422 GPa2% Secant; ASTM D882
Secant Modulus, TD 0.1504 GPa2% Secant; ASTM D882
Impact 10[lbf]; Puncture Resistance Force; Dow Method
 372[ft-lbf/in3]; Puncture Resistance; Dow Method
 2453[ft-lbf/in3]; Toughness MD; ASTM D882
 4321[ft-lbf/in3]; Toughness TD; ASTM D882
Puncture Energy 38.0 in-lbDow Method
Elmendorf Tear Strength MD 224 gMethod B; ASTM D1922
Elmendorf Tear Strength TD 640 gMethod B; ASTM D1922
Elmendorf Tear Strength, MD 280 g/milASTM D1922
Elmendorf Tear Strength, TD 800 g/milASTM D1922
Dart Drop Test <= 100 gMethod B; ASTM D1709
 134 gMethod A; ASTM D1709
Film Tensile Strength at Break, MD 8073 psiASTM D882
Film Tensile Strength at Break, TD 6849 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 123 °CDow Method (DSC)
Vicat Softening Point 99.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %ASTM D1003
Gloss 95 %45°; ASTM D2457
 157 %20°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Cling g218ASTM D5458, unstretched

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin

PDOW1454 / 30672

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.