MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® 2205 Polycarbonate, Injection Grade
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: MVR (300 °C/1.2 kg) 34 cm³/10 min; general purpose; low viscosity; easy release; injection molding - melt temperature 280 - 320 °C; available in transparent, translucent and opaque colors

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.660 g/ccpellets; ISO 60
Density 1.19 g/ccISO 1183-1
Moisture Absorption at Equilibrium 0.12 %50% RH; ISO 62
Water Absorption at Saturation 0.30 %
Water Vapor Transmission 15.0 g/m²/day85 % RH; 100 µm film; ISO 15106-1
Oxygen Transmission 750 cc-mm/m²-24hr-atm[cm³/(m²·24 h·bar)], 100 µm film; b.o. ISO 2556
 3150 cc-mm/m²-24hr-atm[cm³/(m²·24 h·bar)], 25.4 µm (1 mil) film; b.o. ISO 2556
Nitrogen Transmission 150 cc-mm/m²-24hr-atm[cm³/(m²·24 h·bar)], 100 µm film; b.o. ISO 2556
 630 cc-mm/m²-24hr-atm[cm³/(m²·24 h·bar)], 25.4 µm (1 mil) film; b.o. ISO 2556
Carbon Dioxide Transmission 4500 cc-mm/m²-24hr-atm[cm³/(m²·24 h·bar)], 100 µm film; b.o. ISO 2556
 18900 cc-mm/m²-24hr-atm[cm³/(m²·24 h·bar)], 25.4 µm (1 mil) film; b.o. ISO 2556
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmb.o. ISO 25777
Linear Mold Shrinkage, Flow 0.0065 cm/cm60x60x2 mm; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0065 cm/cm60x60x2 mm; 500 bar; ISO 294-4
Melt Flow 37 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 4900 N
@Temperature 23.0 °C
ISO 6603-2
 5900 N
@Temperature -30.0 °C
ISO 6603-2
Ball Indentation Hardness 115 MPaISO 2039-1
Tensile Strength at Break 60.0 MPa50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 65.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %Nominal, 50 mm/min; ISO 527-1,-2
 120 %50 mm/min; ISO 527-1,-2
Elongation at Yield 6.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.40 GPa1 mm/min; ISO 527-1,-2
Flexural Strength 97.0 MPa2 mm/min; ISO 178
Flexural Yield Strength 73.0 MPaat 3.5% strain; 2 mm/min; ISO 178
Flexural Modulus 2.35 GPa2 mm/min; ISO 178
Flexural Strain at Yield 7.1 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -30.0 °C
3 mm, Complete break; ISO 7391/b.o. ISO 180-A
 55.0 kJ/m²
@Temperature 23.0 °C
3 mm, Partial break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1eU
 NB
@Temperature -30.0 °C
ISO 179-1eU
 NB
@Temperature -60.0 °C
ISO 179-1eU
Charpy Impact, Notched 1.20 J/cm²
@Temperature -30.0 °C
3 mm, Complete break; ISO 7391/b.o. ISO 179-1eA
 5.50 J/cm²
@Temperature 23.0 °C
3 mm, Partial break; ISO 7391/b.o. ISO 179-1eA
Puncture Energy 55.0 J
@Temperature 23.0 °C
ISO 6603-2
 60.0 J
@Temperature -30.0 °C
ISO 6603-2
Tensile Creep Modulus, 1 hour 2100 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 1700 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm1 mm; IEC 60243-1
Dissipation Factor 0.00050
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 VCTI M; Solution B; IEC 60112
 250 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Thermal Conductivity 0.200 W/m-KISO 8302
Hot Ball Pressure Test 136 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 137 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 124 °CISO 75-1,-2
Vicat Softening Point 145 °C50 N/50°C/hr; ISO 306
 146 °C
@Load 5.10 kg
120°C/hr; ISO 306
Glass Transition Temp, Tg 145 °CISO 11357-1,-2
UL RTI, Electrical 125 °C
@Thickness 1.50 mm
UL 746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
UL 746B
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.50 mm
UL 746B
Flammability, UL94 HB
@Thickness 2.90 mm
 V-2
@Thickness 0.750 mm
Flash Point 480 °Cignition; ASTM D1929
 550 °Cself ignition; ASTM D1929
Oxygen Index 28 %Method A; IOS 4589-2
Glow Wire Ignition Temperature 875 °C
@Thickness 0.750 mm
IEC 60695-2-13
 875 °C
@Thickness 1.00 mm
IEC 60695-2-13
 875 °C
@Thickness 1.50 mm
IEC 60695-2-13
 875 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 850 °C
@Thickness 0.750 mm
IEC 60695-2-12
 875 °C
@Thickness 1.50 mm
IEC 60695-2-12
 930 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.584Procedure A; ISO 489
Haze <= 0.80 %
@Thickness 3.00 mm
ISO 14782
Transmission, Visible 87 %
@Thickness 4.00 mm
ISO 13468-2
 88 %
@Thickness 3.00 mm
ISO 13468-2
 89 %
@Thickness 1.00 mm
ISO 13468-2
 89 %
@Thickness 2.00 mm
ISO 13468-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection; ISO 294
Mold Temperature 80.0 °CInjection; ISO 294
Injection Velocity 200 mm/secISO 294
 
Descriptive Properties
Electrolytic corrosionA1IEC 60426
Needle flame test10 sMethod K, 3 mm; IEC 60695-11-5
 120 sMethod F, 2 mm; IEC 60695-11-5
 120 sMethod F, 3 mm; IEC 60695-11-5
 5 sMethod K, 1.5 mm; IEC 60695-11-5
 5 sMethod K, 2 mm; IEC 60695-11-5
 60 sMethod F, 1.5 mm; IEC 60695-11-5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2405 Polycarbonate, Injection Grade
Covestro Makrolon® 1260 Polycarbonate, Impact Grade
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Covestro Makrolon® 2858 Polycarbonate, Injection Grade
Covestro Makrolon® 2207 Polycarbonate, Injection Grade

PBA427 / 26928

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.