MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ipiranga Petrochem GP 100 BK HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: The resin GP 100 BK is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal technology, has excellent mechanical properties and very high stress cracking resistance and resistance to internal pressure.

Applications:

  • Pressure pipes for gas distribution

Ipiranga Petrochem polymer product lines have been acquired by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 - 0.962 g/ccASTM D792-00
ESCR 100% Igepal® >= 1000 hourASTM D1693-01
Melt Flow 6.1 - 7.5 g/10 minASTM D1238-04
 0.16 - 0.22 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238-04
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 10.0 MPaISO 9080-03
Flexural Modulus 0.880 GPa
@Strain 2 %
Secant; ASTM D790-02
Izod Impact, Notched 275 J/mASTM D256-03
 
Descriptive Properties
Slow Crack Growth (h)>165

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem GF4950HS HDPE Blow Molding Polyethylene Copolymer
LyondellBasell Alathon® L5906 High Density Polyethylene
Ipiranga Petrochem GP 100 OR HDPE
Baystar™ B5845 High Density Polyethylene - Blow Molding Resin
Braskem BS600 HDPE Blow Molding Polyethylene Copolymer

PIPIRA69 / 48402

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.