MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® A3 GF 30 S1 black 950058 (1365) PA 6.6 Dry, 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: AKROMID A3 GF 30 S1 black 950058 (1365) is a 30% glass fiber reinforced, cold impact strength polyamide 6.6 with high stiffness and strength. Applications are technical parts with high accuracy for engine building and automotive industry.

Features:

  • High Stiffness
  • High Strength
  • Low Temperature Impact Resistance
Uses:
  • Automotive Applications
  • Engineering Parts

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Filler Content 30 %30 %ISO 1172
Moisture Absorption 1.7 %
@Temperature 70.0 °C
1.7 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inISO 294-4
Spiral Flow 69.0 cm27.2 inCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 180 MPa26100 psi5 [mm/min]; ISO 527-2
Elongation at Break 5.0 %5.0 %5 [mm/min]; ISO 527-2
Tensile Modulus 9.60 GPa1390 ksi1 [mm/min]; ISO 527-2
Charpy Impact Unnotched  8.50 J/cm²
@Temperature -30.0 °C
40.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 10.5 J/cm²
@Temperature 23.0 °C
50.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.70 J/cm²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FDIN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FUnannealed; ISO 75/A
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Conditioned, 30% Glass Filled
A-Glass Fiber, Generic
Akro-Plastic Akromid® A3 GF 30 black PA 6.6 Conditioned, 30% Glass Filled
Akro-Plastic Akromid® A3 GF 30 black PA 6.6 Dry, 30% Glass Filled
6060 Aluminum Composition Spec

PAKRO201 / 182788

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.