MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin PW2210 Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM PW2210 resin is an imporved flow 20% glass fiber reinforced amorphous polyetherimide (PEI) resin that is offering a high glass transition temperature (Tg) of 217°C. The material has global food contact compliance (FDA, CN, EC), potable water certifications: NSF 61, KTW-BWGL, EN16421. REG4, ACS, WRAS re-certifications are in progress. Features are excellent mechanical, and dimension properties up to high temperatures also under wet conditions. The material offers very good hydrolytic and chemical resistance for an amorphous material. The material is RoHS compliant. Certified colors are natural (transparent amber) and black.

Features: High Stiffness,Potable Water Certified,Hydrolytic Stability,Chemical Resistance,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.550 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.0 %ISO 62-1
Viscosity 10 cP
@Load 5.00 kg,
Temperature 360 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 150 MPaH358/30; ISO 2039-1
Tensile Strength at Break 140 MPa5 mm/min; ISO 527
Elongation at Break 2.0 %5 mm/min; ISO 527
Tensile Modulus 6800 MPa1 mm/min; ISO 527
Flexural Strength 210 MPabreak, 2mm/min; ISO 178
Flexural Modulus 6500 MPa2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 30.0 kJ/m²80*10*4; ISO 180/1U
 30.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 35.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 35.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²ISO 179/2C
Taber Abrasion, mg/1000 Cycles 17CS-17, 1 kg; SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.280 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 210 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 205 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 212 °CRate B/50; ISO 306
 218 °CRate B/120; ISO 306
 223 °CRate A/50; ISO 306
Oxygen Index 46 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 360 - 410 °C
Zone 2 360 - 410 °C
Zone 3 370 - 420 °C
Melt Temperature 370 - 410 °CInjection Molding
Mold Temperature 140 - 180 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Precipitation Temperature 80.0 - 120 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82751 / 290698

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.