MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC XENOY™ XL1339 PC+PBT (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Data generated in BOZ labs. High heat grade for nonchemical resistance required applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Water Absorption 0.10 %24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.20 %50% RH; ASTM D570
 0.70 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cmSABIC method
Melt Flow 4.0 g/10 min
@Load 1.20 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPa50 mm/min; ISO 527
 49.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 49.0 MPa50 mm/min; ASTM D638
 55.0 MPa50 mm/min; ISO 527
Elongation at Break 70 %50 mm/min; ISO 527
 110 %50 mm/min; ASTM D638
Elongation at Yield 5.0 %50 mm/min; ASTM D638
 5.0 %50 mm/min; ISO 527
Tensile Modulus 2090 MPa50 mm/min; ASTM D638
Flexural Yield Strength 80.0 MPa2 mm/min; ISO 178
 94.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2090 MPa1.3 mm/min, 50 mm span; ASTM D790
 2200 MPa2 mm/min; ISO 178
Poissons Ratio 0.40ASTM E132
Izod Impact, Notched 699 J/mASTM D256
 224 J/m
@Temperature -40.0 °C
ASTM D256
 245 J/m
@Temperature -30.0 °C
ASTM D256
 598 J/m
@Temperature -20.0 °C
ASTM D256
 672 J/m
@Temperature 0.000 °C
ASTM D256
Izod Impact, Notched (ISO) 40.0 kJ/m²80*10*4; ISO 180/1A
 15.0 kJ/m²
@Temperature -40.0 °C
80*10*4; ISO 180/1A
 25.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 35.0 kJ/m²
@Temperature -20.0 °C
80*10*4; ISO 180/1A
 38.0 kJ/m²
@Temperature -10.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 45.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 35.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 16CS-17, 1 kg; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmASTM D257
Dielectric Constant 3.1
@Frequency 1e+6 Hz
ASTM D150
 3.3
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 16.9 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.0020
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.6 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 79.2 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Thermal Conductivity 0.180 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 125 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 105 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 130 °CRate B/50; ISO 306
 135 °CRate B/120; ISO 306
 140 °CRate A/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 255 - 270 °CInjection Molding
Zone 1 245 - 265 °C
Zone 2 250 - 270 °C
Zone 3 255 - 275 °C
Melt Temperature 260 - 275 °C
Mold Temperature 65.0 - 90.0 °C
Drying Temperature 110 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 80 %
Vent Depth 0.00130 - 0.00200 cm
Screw Speed 50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10873 / 244340

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.