MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Accella Bayblock® Primer RI Primer
Categories: Polymer

Material Notes: Bayblock Prime RI is a water-based two component rust inhibitive primer.

Properties / Applications: Bayblock Prime NS is designed for the preparation of surfaces for the application of elastomeric coatings and spray polyurethane foam. This material can be easily sprayed, rolled, or brushed on and provides excellent adhesion to most surfaces. Bayblock Prime NS primer requires minimal set time before foam application. This product is water reducible. Use of Bayblock Prime NS primer in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Covestro sold their spray polyurethane foam business to Accella in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/cc
Solids Content 58 - 62 %by volume
 60 - 64 %by weight
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45ASTM D2240
Impact Test >= 160 in-lbASTM D2794
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air 50.0 °F
 
Processing PropertiesOriginal ValueComments
Pot Life 240 min
 
Descriptive Properties
ColorOrange

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0065 / 201848

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.