MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling Glastic® UTR Polyester Laminate
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: Glastic® UTR offers a superior combination of electrical and mechanical properties. Made from fiberglass-reinforced thermoset polyester resins, these UL®-recognized sheets blend excellent performance characteristics with economy. The numerous property advantages of RGC laminates include:

Electrical Insulation: All electrical insulating laminates have inherently good dielectrics. The grades featured here have been engineered to maximize the specific properties required for a wide range of electrical applications.

Flame Resistance: UTR is UL-rated V-0 and is a halogen free system that generates very low smoke and smoke toxicity in a fire situation.

Mechanical Strength: High impact fiberglass-reinforced polyester laminates won’t shatter. Rigid laminates provide structural support as they insulate. Flexible laminates are available for applications that require a minimum bend radius of 19mm diameter.

Heat Resistance: Glastic® laminates offer excellent property retention and dimensional stability at elevated temperatures. These laminates have UL temperature index ratings from 120 – 210°C electrical, and from 130 –210°C mechanical.

Ease of Fabrication: These materials are easily fabricated with standard metal working equipment. They can be punched, drilled, machined, sheared and sanded. Grade UTR is well known for its ease of fabrication in high-speed machining centers.

Cost Effectiveness: In addition to significant property benefits, Glastic® laminates offer cost effectiveness over most high-pressure laminates. They outperform the phenolic grades and can often replace the more exotic epoxies and silicones at a considerable cost savings.

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.81 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 54.0 MPaParallel; ASTM D638
Flexural Strength 152 MPaPerpendicular; ASTM D790
Compressive Strength 228 MPaPerpendicular; ASTM D695
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 18.0 kV/mm
@Temperature 90.0 °C
Perpendicular, air; ASTM D149
 23.0 kV/mm
@Temperature 90.0 °C
Perpendicular, oil; ASTM D149
 47.0 kV/in
@Temperature 90.0 °C
Parallel; ASTM D149
Comparative Tracking Index 500 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CASTM D696
Thermal Conductivity 0.270 W/m-KASTM C177
UL RTI, Electrical 130 °CUL 746 B
UL RTI, Mechanical without Impact 160 °CUL 746 B
Flammability, UL94 V-0
@Thickness >=2.50 mm
 
Descriptive Properties
Colorwhite/red

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROCH9082 / 232785

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.