MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Nymax™ GMF 604 40 HS Black 124 LW Nylon 6 with 40% Glass\Mineral  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part performance. These materials have been specifically formulated to offer ease of processing in most standard thermoplastic processing equipment.

Property data measured on molded test bars: Dry as Molded

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Filler Content 40 %Glass\Mineral
Water Absorption 0.80 %
@Thickness 0.508 mm,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 121 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 2.0 - 3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 7580 MPaASTM D638
Flexural Strength 186 MPaASTM D790
Flexural Modulus 7580 MPaASTM D790
Izod Impact, Notched 53.4 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 198 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Descriptive Properties
AdditiveHeat Stabilizer
AppearanceBlack
FeaturesGeneral Purpose
 Heat Stabilized
 Low Warpage
FormsPellets
Generic NamePolyamide 6 (Nylon 6)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Nymax™ GMF 604 40 UV Black 28 Polyamide 6 (Nylon 6)
Avient Nymax™ GMF 604 40 UV Black 148 Polyamide 6 (Nylon 6)
Avient Nymax™ GMF 600 P 40 Natural Nylon 6 with 40% Glass\Mineral
Avient Nymax™ GMF 600 A 40 HS Natural Polyamide 6 (Nylon 6)
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled

PH1PN9384 / 103220

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.