MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger XP-151 Compression Molded PI Compound, 15% Graphite Filled, Premium Grade
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes: The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal stability. The bearing grades of the XP 150 Series have excellent wear because of the encapsulated graphite used.

The XP 150 Series of Polyimides are non-melting high temperature materials with high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance along with good chemical resistance.

Typical Applications:

  • Bearings and Bushings
  • Ball Valve Seats
  • Semiconductor Processing Equipment
  • Gears
  • Tanks
  • Electrical Components
  • Pump Parts
  • Hydraulic Components
  • Gaskets
  • Circuit Boards

Information provided by Ensinger Special Polymers, Inc.

Vendors: Ensinger Special Polymers, Inc. provides consistent, high quality compression molded stock shapes of engineering thermoplastics. Common shapes include rings, rods, plates, tubes, and discs. Large diameter rings up to 90" OD are available.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792
Filler Content 15 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 8600 psiASTM D638
Elongation at Break 1.7 %ASTM D638
Tensile Modulus 730000 psiASTM D638
Flexural Strength 14700 psiASTM D790
Flexural Modulus 650000 psiASTM D790
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger XP-132 Compression Molded PI Compound, 15% Graphite Filled
Ensinger TECASINT 8001 Polytetrafluoroethylene (PTFE) + Polyimide, 20% (PI)
Ensinger XP-133 Compression Molded PI Compound, 20% Carbon Fiber
Ensinger XP-154 Compression Molded PI Compound, 40% Graphite, Premium Grade
Hippe PI

PENSIN970 / 140843

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.