MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Denka GR-3500 ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Super high Impact & good flow Grade. Used in a wide range of applications, including toys, home articles, home electric appliances, OA equipment, exterior and interior automotive parts, etc.

Information provided by Denka Company Limited.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccASTM D-792
 1.04 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 2.00 mm
DENKA Method
Melt Flow 14 g/10 min
@Load 9.99 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ISO 2039-2
 109ASTM D-785
Tensile Strength at Break 32.0 MPa50 mm/min; ISO 527-1,-2
 38.0 MPa5 mm/min; ASTM D-638
Tensile Strength, Yield 41.0 MPa50 mm/min; ISO 527-1,-2
Tensile Modulus 2200 MPa1 mm/min; ISO 527-1, -2
Flexural Strength 63.0 MPa15 mm/min; ASTM D-790
 65.0 MPa2 mm/min; ISO 178
Flexural Modulus 2050 MPa2 mm/min; ISO 178
 2150 MPa15 mm/min; ASTM D-790
Izod Impact, Notched 310 J/mASTM D-256
Charpy Impact, Notched 30.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+16 ohm50% RH; JIS K 6911
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °CFlatwise; ISO 75-1, -2
 85.0 °CEdgewise; ASTM D-648
Vicat Softening Point 95.0 °C
@Load 5.10 kg
ISO 306
 95.0 °C
@Load 5.10 kg
ASTM D-1525
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 200 °CCylinder 1
 200 - 230 °CCylinder 2
 210 - 260 °CCylinder 3
Nozzle Temperature 210 - 255 °C
Mold Temperature 40.0 - 60.0 °C
Drying Temperature 80.0 - 85.0 °C
@Time 7200 - 10800 sec
Back Pressure 71.1 - 142 psi
Screw Speed 80 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDENJ809 / 250153

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.