MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
C.O.I.M. FILCO® 650 Film Former for Glass Fiber Sizes
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes: Description: Film Former for Glass Fiber Sizes
General Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.
Typical Physical and Chemical Characteristics: Filco 650 is an unsaturated modified polyester polymer in a non ionic water emulsion.
Characteristics of the dried film:
  • clear
  • non tacky
  • compatible with unsaturated polyester and other thermosets
  • low soluble in styrene

Applications: Filco 650 is suggested as a binder for performs and c.s. mat with low solubility in styrene. The use of organic peroxide as a source of free radicals is suggested. Benzoyl peroxide in water dispersion can for example be used at a level of 0.5 - 1.0% on Filco 650. Filco 650 is also suggested as a film former for glass fiber sizes for:
  • roving for smc
  • bmc

Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 50 - 54 %MA145LFE
Particle Size 1.0 - 2.5 µmMA147LFE
pH 1.5 - 3.5MA148LFE
Viscosity 500 - 2500 cP
@Temperature 25.0 °C
spindle n 3-10 RPM; MA143LFE
 
Descriptive Properties
AppearanceMilky Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
C.O.I.M. FILCO® 300 Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber Sizing
C.O.I.M. FILCO® 362 Film Former for Glass Fiber Sizes
C.O.I.M. FILCO® 350 Non Ionic Unsaturated Polyester Polymer Emulsion for Glass Fiber Sizing
C.O.I.M. FILCO® 309 Film Former for Glass Fiber Sizes
C.O.I.M. FILCO® 306 Film Former for Glass Fiber Sizes

PCOIM111 / 28714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.