MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema OREVAC® 9314 EVA Terpolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as free flowing natural coloured granules. Applications include blown film extrusions, cast film coextrusions, coextrusion tubes, and thermo-adhesive films.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.938 g/ccASTM D1505
Vinyl Acetate Content 13 - 15 %Arkema
Melt Index of Compound 1.5 - 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92ASTM D2240
Tensile Strength at Break 23.0 MPaASTM D638
 25.0 MPaFilm Property, 50 µm thickness; ASTM D882
Tensile Strength, Yield 4.70 MPaASTM D638
 5.50 MPaFilm Property, 50 µm thickness; ASTM D882
Elongation at Break 500 - 700 %Film Property, 50 µm thickness; ASTM D882
 700 - 900 %ASTM D638
Dart Drop Test 365 gASTM D1709
 
Thermal PropertiesOriginal ValueComments
Melting Point 95.0 °CDSC
Vicat Softening Point 71.0 °CASTM D1525
Ring & Ball Softening Point >= 200 °C
 
Optical PropertiesOriginal ValueComments
Haze 4.7 %
@Thickness 0.0500 mm
Film; ASTM D1003
 
Descriptive Properties
MAH Mini800

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema OREVAC® CA 100 Grafted Maleic Anhydride Polypropylene
Arkema OREVAC® PPC Grafted Maleic Anhydride Polypropylene
Arkema Orevac® SM7-001-sPP Maleic Anhydride modified Polypropylene
Arkema OREVAC® 18750 Maleic Anhydride Modified Polypropylene
Arkema Orevac® 18216 Maleic Anhydride modified EVA

PARKG108 / 80126

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.