MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shinil Chemical SHINCON PMMA Electro Conductive Polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's patented conductive filler dispersion technology with variety of engineering polymers and their alloys to impart permanent static dissipative to electrically conductive property to thermoplastics. SHINCON contains multiwall carbon nanotube (MWCNT), carbon black (CB), and carbon fiber (CF) as a conductive filler. SHINCON are used in injection molding, film or sheet extrusion for the applications where the desired level of conductivity and unique mechanical property are important. A wide range of the surface resistaivity is obtained by SHINCON formulations for the parts and devices depending upon customer needs and applications.

    Feature and Benefits
  • Permanent electro conductivity
  • Maintain the physical properties of base resin
  • No particulates (CNT product)
  • Lighter weight
  • Recyclability
  • Easy processing
  • Improved surface
  • Cost effective

Grade/Application: Pelicle box

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 300 kg(f)/cm²
Flexural Strength 44.145 MPa
Flexural Modulus 13000 kg(f)/cm²
Izod Impact, Notched 6.00 kg-cm/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+10 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1899 X 136863 C CLEAR Acrylic (PMMA); Permanently Anti-static - Transparent Grade
Polycasa Acryl® KR 2007/1 Acrylic
Lucite International Elvacite® 2044 Acrylic Resin
Röhm Plexiglas® 99845 Crystal Clear Elastomer Based Film
Polycasa Acryl® KR 2014/1 Acrylic, Impact Grade

PSHINL18 / 104020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.