MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total 3429 Polypropylene, LTHA Injection Molding Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 3289MZ

Applications: ATOFINA 3429 is recommended for appliance parts and is particularly suited for parts that are exposed to hot/wet environments, such as: washing machine, dishwasher and coffee machine parts.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103ASTM D288A
Tensile Strength, Ultimate 4800 psiASTM D638
Elongation at Break 12 %ASTM D638
Tensile Modulus 200000 psiASTM D882
Flexural Modulus 1.24 GPaASTM D790
 180000 psiASTM D 790
Izod Impact, Notched 32.0 J/mASTM D256
Izod Impact, Unnotched 24.0 ft-lb/inASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC-2 Differential Scanning Calorimeter
Deflection Temperature at 0.46 MPa (66 psi) 121 °CASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3429 Polypropylene, Injection Molding Grade
Akro-Plastic Akromid® S3 GF 30 4 black (3429) PA 6.10 Dry, 30% Glass Filled
Total PPC 4624WZ Polypropylene, Impact Copolymer
M. Holland Company MTEGRITY™ CP500 Polypropylene Copolymer
3M 7120 Performance Paper Label Material

PFINAA062 / 38498

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.