MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Nourycryl MA 128 (2,2-pentamethylene-1,3-oxazolidyl-3)ethylmethacrylate
Categories: Other Engineering Material

Material Notes: Nourycryl MA 128 is a methyl acrylate monomer used as a functional building block in polyurethane coatings.

CAS number: 4203-89-8

EINECS/ELINCS No: 224-116-8

Applications: Nourycryl MA 128 containing resins can be applied in urethane systems such as one-pack acrylic/urethane high performance coatings. They provide a long pot-life and short curing times under ambient conditions, while allowing for very high solid contents in durable polyurethane coatings, e.g. used in the aerospace industry.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 - 1.06 g/cc0.0376 - 0.0383 lb/in³
Viscosity 20 cP20 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point >= -15.0 °C>= 5.00 °F
Boiling Point 109 °C
@Pressure 0.00260 MPa
228 °F
@Pressure 0.377 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4845 - 1.48651.4845 - 1.4865
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AppearanceClear to turbid liquid
Assay= 94 %
Color= 5 G
Content= 250-350 mg/kgp-Methoxyphenol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY723 / 286246

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.