MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cri-Tech Cri-plastMP PFA-12xx EC PFA
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Cri-plast MP PFA Electrically Conductive Compounds are formulated to meet your static dissipative/conductive, ATEX requirements in multiple applications. Specific grades can be processed by injection, extrusion, transfer molding, and compression molding.

Special Features:

  • Low Particle Count
  • Excellent electrical, chemical, and thermal performance.
  • Superior blend of physical properties and processability.
  • Unique MFI Flow/MIT Flex performance balance
  • Retains electrical conductivity even at 150% elongation.
  • Retains stable conductivity over the entire PFA service temperature range (260 C).
  • Non-marking due to lower filler loading.
  • Matte surface appearance
Typical applications:
  • Injection molded parts
  • Tubing/Linings
  • Injection/Transfer Molding
  • Sheet/film
Process: Ext/Transfer

Information provided by Cri-Tech, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.14 g/cc2.14 g/ccASTM D-3307
Melt Flow 1.5 - 4.0 g/10 min1.5 - 4.0 g/10 minASTM D-3307
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.193 MPa28.0 psiASTM D-3307
Elongation at Break 240 %240 %ASTM D-3307
 
Thermal PropertiesMetricEnglishComments
Melting Point 300 - 310 °C572 - 590 °FASTM D-3307

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCRITECH088 / 316297

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.