LEXAN HP4 is a medium flow polycarbonate (PC) with an MVR (300°C/1.2kg) of 10. This is a biocompatible (ISO10993 or USP Class VI) grade for medical devices and pharmaceutical applications. It is EtO and steam sterilizable, contains mold release and adheres to our healthcare management of change policy.Information provided by SABIC |