MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bada BADAMID® PA12 CF20/GF10 black S3 PA12, 20/10% Carbon/Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 20% Glass Fiber Filled; Nylon 12, Carbon Fiber Filled

Material Notes: UV-protected polyamide 12 injection molding grade with carbon fiber and glass reinforcement for electrically conductive parts

Information provided by Bada

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPa5 mm/min; ISO 527-1/2
Elongation at Break 4.0 %5 mm/min; ISO 527-1/2
Tensile Modulus 9800 MPa1 mm/min; ISO 527-1/2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 17.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1000 ohm-cmIEC-62631-3-1
Surface Resistance <= 1000 ohmIEC-62631-3-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 178 °C10 K/min; ISO 3146
Maximum Service Temperature, Air 80.0 °C
@Time 7.20e+7 sec
EC-60216
Deflection Temperature at 0.46 MPa (66 psi) 170 °CISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 150 °CISO 75-1/2
Flammability, UL94 HB
@Thickness 0.750 mm
 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °C
Mold Temperature 40.0 - 60.0 °C
Drying Temperature 80.0 °C
Dry Time 4.00 - 8.00 hour
Moisture Content <= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBADA194 / 287027

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.