Hostacom TYS 696N 2065 is an unfilled impact modified polypropylene, with high melt flow rate and high impact resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 2065 color version. Applications: Interior Automotive ApplicationsInformation provided by LyondellBasell. |