Chemical resistance and high impact resistance. Applications: Kitchen and home appliances. POLYLAC® ABS resin is a copolymer primarily composed of styrene (SM), acrylonitrile (AN), and butadiene (BD). ABS has very good mechanical properties, dimensional stability, processing ability, chemical resistance, and a high-quality appearance. Information provided by Chi Mei Corporation |