MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Celanese Celanex® 3105H PBT, 15% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes:

Information provided by Celanese Corporation.

Key Words: 15% glass filled PBT with good toughness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 94.0 MPa5mm/min; ISO 527-2/1A
Elongation at Break 3.8 %5mm/min; ISO 527-2/1A
Tensile Modulus 5470 MPa1mm/min; ISO 527-2/1A
Flexural Strength 138 MPaISO 178
Flexural Modulus 5160 MPaISO 178
Charpy Impact, Notched 4.20 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 224 °CISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 174 °CISO 75-1, -2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 2300 G6 HR BK15116 30% Glass Filled PBT
BLUESTAR PBT 403M-G20 20% Glass Filled
BLUESTAR PBT 6630 30% Glass Filled
DuPont Mobility and Materials Rynite® FR530L NC010 Polyethylene Terephthalate (PET)
Eastman BD445 PET

PHCS035 / 123450

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.