MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
The NanoSteel® Company SHS 9500 GMAW OAW Steel Alloy, Cored Wire
Categories: Metal; Ferrous Metal; Alloy Steel; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Coating Description: SHS 9500 GMAW OAW is an iron based steel alloy featuring medium hardness, high toughness and high wear resistance.

Key Performance Characteristics:

  • 58-62 HRc single and double pass weld deposits
  • Minimal cracking when applied to plain carbon and alloy steels
  • Cost effective: contains no tungsten, molybdenum or nickel
  • High resistance to abrasion and galling
  • SHS GMAW OAW features a unique uniform glass-forming melt chemistry that allows high undercooling to be achieved during welding. This results in considerable refinement of the crystalline microstructure down to a near nanoscale (400 nm length scale) range.

    Application Process: GMAW OAW Weld Overlay for Hardfacing

    Information Provided by The NanoSteel Company, Inc.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 7.59 g/ccWeld Deposit Property
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Rockwell C 58 - 62
     
    Component Elements PropertiesOriginal ValueComments
    Boron, B <= 6.0 %
    Carbon, C <= 3.0 %
    Chromium, Cr <= 10 %
    Iron, Fe >= 65 %
    Manganese, Mn <= 5.0 %
    Niobium, Nb (Columbium, Cb) <= 9.0 %
    Silicon, Si <= 2.0 %
     
    Descriptive Properties
    Impact ResistancePassed multiple impacts at 165 ft-lbsDrop Impact Testing
    Wear Resistance Mass Loss (g)0.19-0.256000 cycles; ASTM G65-04 Procedure A

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    MetalTek MTEK 35-45MA Heat Resistant Stainless Steel
    MetalTek MTEK 221-01 Cast UNS J84090 Martensitic Stainless Steel
    MetalTek J92180 17-4 PH® Precipitation Hardening Steel
    Kennametal Stellite Stellite® 306 Cobalt Alloy
    Kennametal Stellite Stellite® 251 Cobalt Alloy

    NNANO016a / 138453

    Rulon Bearings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.