MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Silres® BS 16 Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® BS 16 is an aqueous solution of potassium methyl siliconate and is used in diluted form for the impregnation of mineral construction materials to make them water-repellent. SILRES® BS 16 develops its water-repellent properties by reaction with atmospheric carbon dioxide (CO2). The active substance formed from the silicone masonry water repellent is polymethylsilicic acid. As with all siliconates, however, SILRES® BS 16 can cause a white deposit on the surface of colored construction materials, or if used outside the application guidelines.

Application: Imparting water repellency to:

  • low-fired clay products immediately after they have been made: e. g. roof tiles, facing bricks, floor tiles, flower pots
  • aerated concrete
  • gypsum and gypsum-based fiber boards
  • light fillers, such as perlite, vermiculites and aerated concrete granules
  • insulating materials

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc
@Pressure 0.1013 MPa
0.0506 lb/in³
@Pressure 14.69 psi
Solids Content 54 %
@Treatment Temp. 150 °C,
Time 3600 sec
54 %
@Treatment Temp. 302 °F,
Time 1.00 hour
1g
pH 13 - 1413 - 14
 
Descriptive Properties
Active ingredients (%)34
Appearanceclear to hazy, colorless
Content (%)20K2O equivalent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9530 / 205059

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.