MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Clyrell 7173 XCP Polypropylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell 7173 XCP is clear polypropylene random copolymer particularly suited for thermoforming/injection blow molding and single or multi layer sheet extrusion. It offers an excellent clarity and gloss and these characteristics may be further enhanced through orientation processes (i.e. injection stretch blow molding). The injection molding applications of the Clyrell 7173 XCP include posts and cups for foodstuff, trays for biscuits and bakery products, caps and closures for cosmetic and toiletry applications. Extruded sheet made of the Clyrell 7173 XCP can be used in stationary folders and for thermoforming articles such as trays for fresh pasta, sweets or biscuits, fruit and vegetable containers and posts for dairy products.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 22.0 MPaASTM D882
Film Elongation at Break, MD 750 %ASTM D 882
Coefficient of Friction 0.50ASTM D 1894
Film Tensile Strength at Break, MD 35.0 MPaASTM D882
1% Secant Modulus, MD 660 MPaASTM D 882
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %
@Thickness 0.0500 mm
ASTM D1003
Gloss 90 %
@Thickness 0.0500 mm
ASTM D 2457
 
Descriptive Properties
Processing MethodCast Film, Double Bubble, Injection Blow Molding, Thermoforming

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Adstif HA 3105 Polypropylene
Dow DX5E66 Polypropylene Homopolymer Resin
Borealis Bormed™ RB801CF Polypropylene Random Copolymer
LyondellBasell Moplen RP310M Polypropylene Copolymer
LyondellBasell Moplen RP2795 Polypropylene Copolymer

PEQT7098 / 218735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.