MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Imerys Barden™ AG-1 Kaolin
Categories: Ceramic; Clay; Kaolin Clay; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Barden R is a Hydrated Aluminum Silicate available as an Air Float Beneficiated Fine Powder. This kaolin product is used as a high surface area “hard” filler for agricultural purposes.

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.60 g/cc2.60 g/cc
Brightness 70 - 80 %70 - 80 %% Reflectance
Oil Absorption 33 - 38 %33 - 38 %g/100g clay
Particle Mesh Size 325 Mesh325 Mesh1% retained
pH 4.0 - 5.54.0 - 5.5
Specific Surface Area 22 - 26 m²/g22 - 26 m²/g
 
Component Elements PropertiesMetricEnglishComments
Al2O3 38.1 %38.1 %
Fe2O3 1.6 %1.6 %
Quartz 1.5 - 3.8 %1.5 - 3.8 %
SiO2 45.1 %45.1 %
 
Descriptive Properties
Colorwhite
Heating Loss (% max as produced)1at 105°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Imerys Barden™ R Kaolin
Imerys Barden™ Kaolin

CIMERY031 / 88381

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.