MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sawbones Solid Rigid Polyurethane Foam 10 pcf Density
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Solid Rigid Polyurethane Foam

Primary Use
Solid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mechanical properties of human bone, however, it does provide consistent and uniform material with properties in the range of human cancellous bone. Relevant mechanical properties for comparison to human cancellous bone may depend on the particular test method that is being developed.

The ASTM F-1839-08 "Standard Specification for Rigid Polyurethane Foam for Use as a Standard Material for Testing Orthopaedic Devices and Instruments" states that, "The uniformity and consistent properties of rigid polyurethane foam make it an ideal material for comparative testing of bones screws and other medical devices and instruments."

Description
Solid rigid polyurethane foam has a closed cell content ranging from 96.0 to 99.9%. Foam is available in a range of sizes and densities, from 0.08 to 0.80 grams per cubic centimeter (5 to 50 pounds per cubic foot).
.
Standard block size: 13cm X 18cm X 4cm
Standard sheet size: 13cm X 18cm X 3mm

Other Notes
Water absorption ranges from 0.301 to 0.0 kg/m2
Foam meets ASTM F-1839-08. Block dimensions are within ±2mm and sheet thickness is within ±0.3mm. Foam density may vary ±10%.
Properties parallel to direction of the rise of foam.

Information provided by Sawbones.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.160 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2.10 MPa
Tensile Modulus 0.0860 GPa
Compressive Yield Strength 2.20 MPa
Compressive Modulus 0.0580 GPa
Poissons Ratio 0.30Calculated
Shear Modulus 0.0190 GPa
Shear Strength 1.60 MPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 63.0 µm/m-°C
@Temperature -46.0 - 93.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sawbones Solid Rigid Polyurethane Foam 20 pcf Density
Sawbones Solid Rigid Polyurethane Foam 15 pcf Density
Sawbones Solid Rigid Polyurethane Foam 30 pcf Density
Sawbones Solid Rigid Polyurethane Foam 50 pcf Density
Sawbones Solid Rigid Polyurethane Foam 5 pcf Density

PSAWBO10 / 66541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.