MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODACAL® DSB Surfactant
Categories: Fluid

Material Notes: Identification: SODIUM ALKYL DIPHENYL OXIDE SULFONATE

CAS: 28519-02-0

Polarity: Strongly Anionic

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODACAL DBS is producer ABS type resins and various latex. It is used as Polymerization surfactant. In Oilfield it’s strongly anionic temperature is a stable foam booster.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/cc
pH 7.5 - 8.510% Solution; RP-0420
Viscosity 145 cP
Molecular Weight 569 g/mol
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 8.0RP-0138
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 55 %RP-1450
 
Descriptive Properties
AppearanceClear, Straw Yellow Liquid
CompositionActive>45%, 100%-Water-Salts-Free Oil
 Petroleum Ether Extract<1.0%, RP-0210
 Total Salt (NACL+NA2SO4)<1.0%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODACAL® DS-4 Surfactant
Solvay RHODACAL® N Surfactant
Solvay IGEPAL® CO 897 Surfactant
Solvay RHODACAL® SS-45/A2 Surfactant
Solvay RHODACAL® SSA/A Surfactant

WRHOD338 / 137569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.