MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Chesterton ARC T7 AR Ceramic-Filled Industrial Barrier Coating
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: A novolac vinyl ester based, protective barrier coating for high temperature, chemical exposures where aggressive chemicals and abrasive conditions may be present.

ARC T7 AR industrial coating is designed to: Resist a wide range of inorganic, as well as organic acids and hydrocarbon based chemical compounds; Resist abrasion; Easily apply by trowel

Filler: A proprietary blend of high purity alumina ceramic reinforcements for resistance to sliding abrasion. Matrix: A flexibilized epoxy novolac vinyl ester resin reacted with a cumene hydrogen peroxide catalyst

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/ccCured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 80ASTM D2240
Flexural Strength 3250 psiASTM D790
Flexural Modulus 1.40e+6 psiASTM C580
Compressive Strength 10410 psiASTM D695
Adhesive Bond Strength 2249 psiPull-Off Adhesion; ASTM D4541
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 135 °CWet Service
 180 °CDry Service
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 10.0 - 32.0 °C
Dry, Unopened Containers
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTCHS037e / 239858

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.