MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound DX13354 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DX13354 compound is based on Polycarbonate (PC) resin containing 30% glass fiber. Added features of this grade include: Improved Plating Surface and Mechanical Performance suitable for Laser Direct Structuring (LDS) applications, Improved Impact, Good Surface Aesthetics and Wide Processing Window.

Features: Aesthetics and Appearance,Enhanced Ductility,Laser Direct Structuring,Circuit Solution

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/ccASTM D792
Viscosity 13 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ASTM D1238
Linear Mold Shrinkage, Flow 0.00050 - 0.0010 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 280 °C
ASTM D1238
 16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 27 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPa5 mm/min; ASTM D638
 120 MPa50 mm/min; ISO 527
Elongation at Break 2.4 %5 mm/min; ASTM D638
 2.4 %50 mm/min; ISO 527
Tensile Modulus 8760 MPa5 mm/min; ASTM D638
 8840 MPa1 mm/min; ISO 527
Flexural Strength 170 MPaASTM D790
 180 MPaISO 178
Flexural Modulus 8020 MPaASTM D790
 8450 MPaISO 178
Izod Impact Notched 150 JASTM D256
Izod Impact, Unnotched 700 J/mASTM D4812
Izod Impact, Notched (ISO) 14.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²80*10*4; ISO 180/1U
Charpy Impact Unnotched 50.0 kJ/m²ISO 179/2C
Charpy Impact, Notched 14.0 kJ/m²ISO 179/2C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.44
@Frequency 1.90e+9 Hz
SABIC method
 3.51
@Frequency 5.00e+9 Hz
SABIC method
 3.52
@Frequency 1.10e+9 Hz
SABIC method
Dissipation Factor 0.012
@Frequency 5.00e+9 Hz
SABIC method
 0.013
@Frequency 1.90e+9 Hz
SABIC method
 0.014
@Frequency 1.10e+9 Hz
SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 21.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 69.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 71.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 127 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 126 °C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 124 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 122 °C
@Thickness 3.20 mm
ASTM D648
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 270 - 295 °C
Zone 2 270 - 295 °C
Zone 3 270 - 295 °C
Melt Temperature 270 - 295 °CInjection Molding
Mold Temperature 100 - 120 °C
Drying Temperature 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81564 / 289511

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.