MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES Electrablend® PC SS15 15% Stainless Steel Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Stainless Steel Fiber

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Stainless Steel Fiber, 15% Filler by Weight

Features: Electromagnetic Shielding (EMI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccASTM D792
Water Absorption 0.12 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 10000 psiASTM D638
Elongation at Break 3.0 %ASTM D638
Flexural Strength 12000 psiASTM D790
Flexural Modulus 420000 psiASTM D790
Izod Impact, Notched 1.20 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 21.0 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10 - 1000 ohm-cmASTM D257
Surface Resistance 100 - 1.00e+6 ohmASTM D257
Shielding Effectiveness 55 dB
@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 32.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 295 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 285 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 303V-6 Polycarbonate Resin
Celanese Nilit FRIANYL B63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled
Covestro Makrolon® 2807 MAS 167 Polycarbonate
Covestro Makrolon® 1837 MAS081 Polycarbonate

PTPC1032 / 136970

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.