MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LEXAN™ Copolymer EXL9112 Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.150 %0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %0.35 %ISO 62-1
Viscosity 16 cP
@Load 1.20 kg,
Temperature 300 °C
16 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 17 g/10 min
@Load 1.20 kg,
Temperature 300 °C
17 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 95.0 MPa13800 psiH358/30; ISO 2039-1
Tensile Strength at Break 55.0 MPa7980 psi50 mm/min; ISO 527
 58.0 MPa8410 psi50 mm/min; ASTM D638
Tensile Strength, Yield 58.0 MPa8410 psi50 mm/min; ASTM D638
 59.0 MPa8560 psi50 mm/min; ISO 527
Elongation at Break 100 %100 %50 mm/min; ISO 527
 103 %103 %50 mm/min; ASTM D638
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527
 5.8 %5.8 %50 mm/min; ASTM D638
Tensile Modulus 2.20 GPa319 ksi1 mm/min; ISO 527
 2.26 GPa328 ksi50 mm/min; ASTM D638
Flexural Strength 88.0 MPa12800 psiyield, 2 mm/min; ISO 178
 95.0 MPa13800 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.30 GPa334 ksi2 mm/min; ISO 178
 2.33 GPa338 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 731 J539 ft-lbASTM D256
 560 J
@Temperature -30.0 °C
413 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 53.0 kJ/m²25.2 ft-lb/in²80*10*4; ISO 180/1A
 55.0 kJ/m²26.2 ft-lb/in²80*10*3; ISO 180/1A
 18.0 kJ/m²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
 20.0 kJ/m²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact, Notched 6.00 J/cm²28.6 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 2.50 J/cm²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 67.0 J49.4 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
IEC 60250
 2.7
@Frequency 50.0 - 60.0 Hz
2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 19.0 kV/mm
@Thickness 3.20 mm
483 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor  0.00040
@Frequency 50.0 - 60.0 Hz
0.00040
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 V175 VIEC 60112
 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=0.800 mm
15 - 30 sec
@Thickness >=0.0315 in
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
30 - 60 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI  15 - 30 arcs
@Thickness >=0.800 mm
15 - 30 arcs
@Thickness >=0.0315 in
UL 746A
 >= 120 arcs
@Thickness >=1.50 mm
>= 120 arcs
@Thickness >=0.0591 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  72.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
40.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 75.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow  72.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
40.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 75.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °C277 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 136 °C
@Thickness 3.20 mm
277 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 124 °C255 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 123 °C
@Thickness 3.20 mm
253 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 143 °C289 °FRate B/50; ASTM D1525
 143 °C289 °FRate B/50; ISO 306
 144 °C291 °FRate B/120; ISO 306
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 120 °C248 °FUL 746B
UL RTI, Mechanical without Impact 130 °C266 °FUL 746B
Flammability, UL94  HB
@Thickness >=0.800 mm
HB
@Thickness >=0.0315 in
UL 94
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 5VB
@Thickness >=2.50 mm
5VB
@Thickness >=0.0984 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
Oxygen Index 40 %40 %ISO 4589
Glow Wire Ignition Temperature  825 °C
@Thickness 1.00 mm
1520 °F
@Thickness 0.0394 in
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-13
 825 °C
@Thickness 2.00 mm
1520 °F
@Thickness 0.0787 in
IEC 60695-2-13
 825 °C
@Thickness 2.50 mm
1520 °F
@Thickness 0.0984 in
IEC 60695-2-13
 825 °C
@Thickness 3.00 mm
1520 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 960 °C
@Thickness 2.50 mm
1760 °F
@Thickness 0.0984 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 310 °C554 - 590 °F
Zone 2 280 - 305 °C536 - 581 °F
Zone 3 295 - 315 °C563 - 599 °F
Melt Temperature 295 - 315 °C563 - 599 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80222 / 288169

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.