MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Tin Zinc Alloy, UNS C83470, M01 Temper, As Die Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Sand Cast

Fabrication Properties: Excellent Suitability – Brazing, Carbon Arc Welding; Good Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding

Applicable Specifications: As Continuous Cast- ASTM B505/B505M; As Sand Cast – ASTM B584, Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.69 g/cc0.314 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 193 MPa>= 28000 psi
 248 MPa36000 psiTypical
Tensile Strength, Yield 131 MPa19000 psi0.2% Offset
Elongation at Break >= 15 %>= 15 %
Machinability 75 %75 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000104 ohm-cm0.0000104 ohm-cm16.5% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.7 µm/m-°C
@Temperature 20.0 - 100 °C
10.4 µin/in-°F
@Temperature 68.0 - 212 °F
Melting Point 982 - 1027 °C1800 - 1881 °F
Solidus 982 °C1800 °F
Liquidus 1027 °C1881 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.010 %<= 0.010 %
Antimony, Sb <= 0.20 %<= 0.20 %
Copper, Cu 90 - 96 %90 - 96 %
Iron, Fe <= 0.50 %<= 0.50 %
Lead, Pb <= 0.090 %<= 0.090 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.10 %<= 0.10 %
Silicon, Si 0.20 - 0.60 %0.20 - 0.60 %
Sulfur, S 0.20 - 0.60 %0.20 - 0.60 %
Tin, Sn 3.0 - 5.0 %3.0 - 5.0 %
Zinc, Zn 1.0 - 3.0 %1.0 - 3.0 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC83470x1 / 292534

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.