MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP 3501 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easily mixed to produce strong, impact-resistant bonds.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity >= 1.00e+6 cPRVF, #7 spindle, 2 rpm at RT
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 80
Shear Strength 400 psiOverlap on Etched Aluminum, cured for 20 mins @ RT; ASTM D1002
 500 psiOverlap on Etched Aluminum, cured for 30 mins @ RT; ASTM D1002
 750 psiOverlap on Etched Aluminum, cured for 60 mins @ RT; ASTM D1002
 900 psiOverlap on Etched Aluminum, cured for 90 mins @ RT; ASTM D1002
 1810 psiOverlap on Etched Aluminum, Tap Water @ RT for 14 days; ASTM D1002
 1895 psiOverlap on Etched Aluminum, Salt Spray @ 35°C for 14 days; ASTM D1002
 2030 psiOverlap on Etched Aluminum, 100% RH @ 49°C for 14 days; ASTM D1002
 150 psi
@Temperature 82.0 °C
Steel Overlap; ASTM D1002
 300 psi
@Temperature 82.0 °C
Aluminum Overlap; ASTM D1002
 1000 psi
@Temperature -55.0 °C
Steel Overlap; ASTM D1002
 1500 psi
@Temperature -55.0 °C
Aluminum Overlap; ASTM D1002
 2000 psi
@Temperature 24.0 °C
Steel Overlap; ASTM D1002
 2400 psi
@Temperature 24.0 °C
Aluminum Overlap; ASTM D1002
Peel Strength 4.00 pliAluminum T-Peel; ASTM D1876
 10.0 pliSteel T-Peel; ASTM D1876
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.20e+13 ohm-cm
Dielectric Strength 700 kV/in
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature -50.0 - 10.0 °C
 234 µm/m-°C
@Temperature 50.0 - 110 °C
Thermal Conductivity 2.32 BTU-in/hr-ft²-°F
 
Descriptive Properties
AppearanceBlackAccelerator
 Gray
 WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2086 One-Part Epoxy Adhesives and Metal Primer
Henkel Hysol EA 9330 Paste Adhesive System
Henkel Hysol EA 9686 Film Adhesive
3M Scotch-Weld™ DP270 Black Structural Adhesive
3M Scotch-Weld™ DP-190 Gray Adhesive in Duo-Pak Cartridges

PMM34640 / 169387

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.