MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 516H02 Fiber Optic Adhesive
Categories: Polymer; Adhesive; Thermoset; Filled/Reinforced Thermoset

Material Notes: TRA-BOND 516H02 is a low viscosity, room temperature or low temperature curing fiber optic adhesive with good stress relief, high adhesion, and low shrinkage upon cure. TRA-BOND 516H02 contains very fine filler (< 1 micron) for low CTE and aids in maintaining fiber alignment.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccCured
Viscosity 4000 cPMixed (cp #40, 2.5 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81Overnight @ RT
Adhesive Bond Strength 3900 psiLap shear, alum to alum, 1 hr @ 65°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 48.0 µm/m-°C
@Temperature 20.0 °C
Alpha 1
Glass Transition Temp, Tg 50.0 °CUltimate Tg; TMA
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 - 36.0 hourAt RT
 1.00 hour
@Temperature 65.0 °C
 3.00 - 4.00 hour
@Temperature 40.0 °C
Pot Life 25 min
 
Descriptive Properties
Color ClearHardener
 TanResin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
E-Glass Fiber, Generic
S-Glass Fiber, Generic
RTP Company RTP 4201 Thermoplastic Polyimide (TPI), Glass Fiber
RTP Company RTP 4201 TFE 5 Thermoplastic Polyimide (TPI), Glass Fiber - PTFE Lubricated
NextGen Adhesives P907-04 Fiber Optic Adhesive

PTRAC122 / 71050

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.