MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kraton® D4150 K (O/E SBS) Linear Triblock Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified:
Kraton D4150 KT - supplied as a dusted porous pellet
Kraton D4150 KU - supplied as an undusted porous pellet

Region: North America, Europe, Asia Pacific, Japan, and South America

Uses: Kraton D4150 K is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications, molded and extruded goods applications and may be used in formulating adhesives, sealants, and coatings.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D4025
Volatiles <= 0.70 %<= 0.70 %KM 04
Viscosity 850 cP850 cP25% Toluene Solution at 25°C; BAM 922
Melt Flow 9.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
9.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Ash 0.25 - 0.45 %0.25 - 0.45 %Talc specification for D4150 KT; BAM 908
 
Chemical PropertiesMetricEnglishComments
Diblock Content 17 %17 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 45
@Time 10.0 sec
45
@Time 0.00278 hour
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 19.3 MPa2800 psiMeasured on films cast from a solution in toluene; ASTM D412
Elongation at Break 1400 %1400 %Measured on films cast from a solution in toluene; ASTM D412
300% Modulus 1.103 MPa
@Strain 300 %
160.0 psi
@Strain 300 %
film cast from poluene solution; ASTM D412
 
Descriptive Properties
ContentAntioxidant0.13-0.35%, KM 08
 Oil32.3-34.3%, KM 05
 Polystyrene29-30%, KM 03
Styrene/Rubber Ratio31/69

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® D2122 DO (SBS) Compound
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer
Kraton® D1160 E (SIS) Linear Triblock Copolymer
Kraton® D1161 J (SIS) Linear Triblock Copolymer

PKRA9844 / 132743

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.