MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Garlock GYLON® HP3562 PTFE Gasketing, Steel Insert, Oxygen Service
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Gylon® with perforated 316LSS insert - Oxygen service
  • Perforated stainless steel core increases resistance to pressure fluctuations and thermal cycling
  • GYLON® offers superior cold flow and creep resistance, eliminating the need for frequent retorquing
  • Seals aggressive chemicals in hostile environments where safety or blowout resistance is crucial
Media: Strong acids (except hydrofluoric), Solvents, Hydrocarbons, Water, Steam, Chlorine, Cryogenics

Information provided by Garlock Rubber Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Permeability 0.0150.015Gas Permeability, cc/min; DIN 3535 Part 4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 34.5 MPa5000 psiacross grain; ASTM F152
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C
@Pressure 17.2 MPa
500 °F
@Pressure 2500 psi
Continuous
 
Descriptive Properties
Compressibility, %4-9ASTM F36
Creep Relaxation, %20ASTM F38
Sealability ASTM F37B, ml/hr0.2ASTM Fuel A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGARL824 / 157522

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.