MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Cerafiber® Refractory Ceramic Fiber Bulks Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Cerafiber® Bulk is produced from a high purity blend of alumina and silica by fiberization of melt by the spinning process, as are all “Cera” fibers. Cerafiber Bulks is rated to 2400°F (1315°C).

Applications:

  • Expansion joints
  • Low mass kiln cars
  • Tube seal fabrication
  • Thermal and acoustical insulation
  • Filtration media
  • Reinforcement and filler for plastics, resins and paints
  • Fillers for mastics, cements and vacuum formed boards and shapes

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.08 J/g-°C
Maximum Service Temperature, Air 1177 °CContinuous Use
 
Component Elements PropertiesOriginal ValueComments
Al2O3 46 %after firing
SiO2 54 %after firing
 
Descriptive Properties
Classification Temperature (°C)1315
Colorwhite
Fiber Index45-55%111 Grade
 45-55%112 Grade
 50%HM-12 Grade
 50%HM-25 Grade
 50%HM-50 Grade
Fiber Length13-250 mm
 13mm
 25mm
 50mm
 up to 250mm
 up to 250mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Morgan Advanced Ceramics Ceramic Fiber Blankets Cerawool Blanket
Morgan Advanced Ceramics Ceraform 250 Ceramic Fiber
Morgan Advanced Ceramics Cerafibre® Bulk Thermal Ceramic
Morgan Advanced Ceramics Cerachrome® Refractory Ceramic Fiber Bulks Thermal Ceramic

CMORF7041 / 203340

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.