MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kaowool Ceramic Felt 1260 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Kaowool 1260 Ceramic Felt is manufactured from high purity refractory fibers and designed for high temperature insulation up to 1260°C with a minimum addition of carefully selected bonds. Advanced production techniques ensure uniform fiber distribution and close control of thickness and density. Kaowool 1260 Ceramic Felt exhibits excellent strength, has good flexibility and is pleasant to handle, cuts cleanly and is ideally suited for the manufacture of the most intricate die cut shapes and gaskets, even in thin section, and is available in roll form which permits maximum material utilization offering improved flexibility to the die cutter. Other beneficial properties include low thermal conductivity, low thermal mass and exceptionally high thermal shock resistance.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.130 - 0.190 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 0.550 MPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 1760 °C
Shrinkage 3.5 %
@Temperature 1400 °C,
Time 14400 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 46 - 52 %
Loss on Ignition(%) 7.0 %
Other <= 0.50 %trace organics
SiO2 48 - 54 %
 
Descriptive Properties
Classification Temperature (°C)1260
Colorwhite
Fiber Diameter2-3 µm
Indicative Heat Loss1730.9 ambient, 27°C, still air, at 9mm and 500°C
 2050.9 ambient, 27°C, still air, at 6mm and 500°C
 2500.9 ambient, 27°C, still air, at 3mm and 500°C
 2640.9 ambient, 27°C, still air, at 9 mm and 750°C
 3150.9 ambient, 27°C, still air, at 6 mm and 750°C
 3500.9 ambient, 27°C, still air, at 9 mm and 100°C
 3850.9 ambient, 27°C, still air, at 3mm and 750°C
 4150.9 ambient, 27°C, still air, at 6mm and 1000°C
 4490.9 ambient, 27°C, still air, at 9 mm and 1250°C
 4950.9 ambient, 27°C, still air, at 3mm and 1000°C
 5250.9 ambient, 27°C, still air, at 6mm and 1250°C
Thickness measurement pressure10 kPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese VECTRA B130 LCP, 30% Glass Reinforced (with extra stress-strain data)
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Morgan Advanced Ceramics Kaowool HD Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool PM Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics MAFTEC Blanket

CMORF7084 / 203382

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.