RA130E-2492 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is dark blue colored. Applications: domestic water, heating, relining, plumbing, and industrial applications. The product is used for single as well as for multilayer pipes, where you then differentiate between plastic multilayer and aluminum multilayer pipes. Specifications: DIN 8078; DIN 8077; and EN ISO 15874.Information provided by Borealis AG |