MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow DGDA-2475 NT High Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in corrugated pipe applications. It has been specifically designed for extrusion of corrugated pipes with the addition of color concentrates.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9525 g/ccASTM D792
Environmental Stress Crack Resistance 48 hourF0; Compression molded parts prepared according to ASTM D 1928, condition B.; ASTM D1693
High Load Melt Index 21 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Melt Index of Compound 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62Compression molded parts per ASTM D 1928 Procedure C.; ASTM D2240
Tensile Strength at Break 4600 psiCompression molded parts per ASTM D 1928 Procedure C.; ASTM D638
Tensile Strength, Yield 3500 psiCompression molded parts per ASTM D 1928 Procedure C.; ASTM D638
Elongation at Break 800 %Compression molded parts per ASTM D 1928 Procedure C.; ASTM D638
Flexural Modulus 140000 psiCompression molded parts prepared according to ASTM D 1928, method 1, procedure B.; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -94.0 °FCompression molded parts prepared according to ASTM D 1928, procedure A.; ASTM D746
 
Descriptive Properties
Notched Constant Ligament Stress hours, min24ASTM F2136

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DMDA-8007 NT 7 High Density Polyethylene Resin
Dow DMDA-8907 NT 7 High Density Polyethylene Resin
Chevron Phillips Marlex® 9005 HDPE Injection Molding Resin
Dow DFDC-7525 NT High Density Polyethylene Resin
Dow DGDB-2480 NT High Density Polyethylene Resin

PDOW1258 / 30476

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.