MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kuraray Genestar™ G1500A-M61 Nylon, 50% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: 50% Glass reinforced injection grade.

Main Features:

  • High strength
  • Heat resistance

Examples of applications:

  • Structural parts
  • Steel alternating parts

Key Words: PA9T
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.58 g/cc
Density 1.58 g/ccISO 1183
Water Absorption 0.13 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 250 MPaISO 527-1/-2
Elongation at Break 2.0 %ISO 527-1/-2
Tensile Modulus 16400 MPaISO 527-1/-2
Flexural Strength 370 MPaISO 178
Flexural Modulus 15300 MPaISO 178
Charpy Impact, Notched 17.0 kJ/m²ISO 179/1eA
Coefficient of Friction 0.30ISO JIS K7218-A
K Factor (Wear Factor) 60[mg]
Limiting Pressure Velocity 1.00 MPa-m/sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 16.0 µm/m-°CASTM D696
CTE, linear, Transverse to Flow 36.0 µm/m-°CASTM D696
Melting Point 300 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 275 °CISO 75-1/-2
Glass Transition Temp, Tg 125 °C10°C/min; ISO 11357-1/-2
 
Descriptive Properties
AdditivesRelease Agent
ApplicationsAutomotive
 General Purpose
Chemical ResistanceAcid Resistance
 Alkali Resistance
 Environmental Stress Crack Resistance
 General Chemical Resistance
 Grease Resistance
 Hydrolytically Stable
 Oil Resistance
 Solvent Resistance
Delivery FormBlack
Other FeaturesBarrier Properties
 Creep Resistance
 High Crystallinity
 Thermal Stability
 Weldable
Regional AvailabilityAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America
Special CharacteristicsHeat Stabilized or Stable to Heat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kuraray Genestar™ GX1500A-M41 Nylon, 50% Glass Filled
Kuraray Genestar™ G1352A-M41 Nylon, 35% Glass Filled
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled
Techmer ES HiFill® HTN GF HS L High Temp Nylon 50% Glass Filled
Overview of materials for Nylon 66, 50% Glass Fiber Filled

PKUR109 / 162498

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.