MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik DYNAPOL® L 912 Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: These coating raw materials are suitable for the production of coatings with very good adhesion offering an optimum of elasticity and formability together with an excellent surface hardness. For this reason, lacquers based on DYNAPOL® have proved particularly suitable for stampable and deep drawable coatings. A wide range of products is available for various requirements of the paint and coating industry. DYNAPOL® polyester resins are mainly used for stoving enamels in combination with amino resins. Special properties, such as chemical resistance, weathering resistance and elasticity, can be improved by using blocked polyisocyanate resins. Stoving enamels based on high-molecular copolyesters show particularly good mechanical properties. Medium and low-molecular polyester resins containing more hydroxyl groups are suitable for the manufacture of stoving enamels with good reactivity and high solids content. In combination with high-molecular copolyesters the quality of films can be optimized.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Test 55 cm³/g
Molecular Weight 15000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 3.0[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 105 °C
 
Descriptive Properties
Hydroxyl Number (mg KOH/g)5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik DYNAPOL® L 411 Polyester Resin
Evonik DYNAPOL® S 1402 Linear Copolyester
Evonik DYNAPOL® LH 815 Polyester Resin
Evonik DYNAPOL® 1203 Polyester Resin
SSAB Tunnplat Dogal F40 Metal-coated Mild Steel

PHUMB246 / 81248

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.