MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® 909 BK Flame Retardant Nylon 66/6, 25% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Vydyne 909 is an halogenated, 25% glass filled, flame retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters Laboratories UL 94 flammability classification of V-0 at 0.4mm (0.016") thick.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccISO 1183
Water Absorption 0.70 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 1.3 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 90.0 MPaConditioned; ISO 527-2
 132 MPaDry; ISO 527-2
Elongation at Break 2.2 %Dry; ISO 527-2
 3.0 %Conditioned; ISO 527-2
Tensile Modulus 7100 MPaConditioned; ISO 527-2
 9100 MPaDry; ISO 527-2
Flexural Strength 140 MPaConditioned; ISO 178
 193 MPaDry; ISO 178
Flexural Modulus 5000 MPaConditioned; ISO 178
 8300 MPaDry; ISO 178
Poissons Ratio 0.40Dry; ISO 527-2
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 180
Charpy Impact Unnotched 35.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 40.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 9.40 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 9.50 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
PLC 6; ASTM D495
Comparative Tracking Index 250 - 399 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI >= 120 sec
@Thickness 0.750 mm
PLC 0; UL 746
 >= 120 sec
@Thickness 1.50 mm
PLC 0; UL 746
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.750 mm
PLC 0; UL 746
 >= 120 arcs
@Thickness 1.50 mm
PLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minPLC 3; UL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-2
Melting Point 250 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 230 °CISO 75-2/A
UL RTI, Electrical 65.0 °CUL 746
 130 °C
@Thickness 0.750 mm
UL 746
 130 °C
@Thickness 1.50 mm
UL 746
 130 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.400 mm
UL 746
 65.0 °C
@Thickness 0.750 mm
UL 746
 95.0 °C
@Thickness 1.50 mm
UL 746
 95.0 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 0.400 mm
UL 746
 110 °C
@Thickness 0.750 mm
UL 746
 110 °C
@Thickness 1.50 mm
UL 746
 110 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 0.400 mm
 V-0
@Thickness 0.750 mm
 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 5VA
@Thickness 3.00 mm
 5VA
@Thickness 1.50 mm
Oxygen Index 32 %ISO 4589-1/-2
Glow Wire Ignition Temperature 750 °C
@Thickness 0.750 mm
IEC 60695-2-13
 750 °C
@Thickness 1.50 mm
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
IEC 60695-2-13
 930 °C
@Thickness 0.400 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.400 mm
IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 240 - 270 °CInjection Molding
Middle Barrel Temperature 240 - 270 °CInjection Molding
Front Barrel Temperature 240 - 270 °CInjection Molding
Nozzle Temperature 240 - 270 °CInjection Molding
Melt Temperature 250 - 270 °CInjection Molding
Mold Temperature 65.0 - 95.0 °CInjection Molding
Drying Temperature 80.0 °C
@Time 14400 sec
Injection Molding
 
Descriptive Properties
Automotive SpecificationsDelphi M6538V
 GM GMP.PA66.058
FeaturesFlame Retardant
 Good Crack Resistance
 Good Mold Release
 Good Toughness
 Halogenated
 High Rigidity
 High Strength
 Ignition Resistant
 Lubricated
Suggested Max Regrind (%)25
UsesAppliances
 Automotive Electronics
 Bobbins
 Circuit Boards, Printed
 Connectors
 Electrical Parts
 Electrical/Electronic Applications
 Fasteners
 Hinges, Living
 Housing, Electrical
 Industrial Applications
 Lighting Applications
 Switches

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Stanyl® TW200F6 PA46-GF30, Conditioned, 30% Glass Filled, Heat Stabilized
Envalior Stanyl® TW241F12 PA46-GF60, Conditioned, 60% Glass Filled, Heat Stabilized
BASF Ultramid® A3WG6 30% Glass Filled PA66 (Dry)
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry)
DuPont Mobility and Materials Delrin® 500P BK602 POM

PZASCE9721 / 220824

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.