MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LNP STARAMIDE PF-100-10 HS NAT95 Polyamide 6, Glass Fiber Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Natural color appearance

  • Features: Heat Stabilized
  • Forms: Pellets
  • Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccISO 1183
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmISO294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 205 MPaISO 527-1, -2
Elongation at Break 3.0 %ISO 527-1, -2
Tensile Modulus 14.0 GPaISO 527-1, -2
Flexural Strength 280 MPaISO 178
Flexural Modulus 12.0 GPaISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 90.0 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 215 °CUnannealed; ISO 75A-1, -2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 252 - 266 °C
Mold Temperature 54.4 - 93.3 °C
Drying Temperature 82.2 °C
Dry Time 4 hour
Moisture Content 0.020 %Suggested
Back Pressure 0.172 - 0.345 MPa
 
Descriptive Properties
ColorNatural

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 300 AR 15 TFE 10  Polycarbonate (PC) Aramid Fiber 15% - PTFE 10%
RTP Company RTP 1482 AR 10  Polyethersulfone (PES) Carbon Fiber 15% - Aramid Fiber 10%
LNP Lubricomp® RA-1003 Polyamide 66, Aramid Fiber Reinforced
RTP Company RTP 300 AR 15 TFE 15 SI  Polycarbonate (PC) Aramid Fiber 15% - PTFE 15% - Silicone
LNP Lubricomp® PDX-E-00548 CCS Polyetherimide, Aramid Fiber Reinforced, PTFE Lubricant

PZLNP1280 / 51362

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.