MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Oroglas® V 825 T Acrylic  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: OROGLAS V 825 T exhibits an excellent balance of properties including superior thermal resistance with an easy processing behavior.

OROGLAS V 825 T is then the material of choice for automotive application like: tail lamp, signal lenses, light guides and cluster lenses.

The OROGLAS V 825 T LI version was developed in order to improve processing and easy demolding

The OROGLAS V 825 T FGL version is designed for food contact applications.

ISO data provided by the manufacturer, Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/cc
Water Absorption 1.9 %
Moisture Absorption at Equilibrium 0.30 %Humidity Absorption
Melt Flow 2.8 g/10 min
@Load 3.80 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 85.0 MPa50 mm/min
Elongation at Break 6.0 %Nominal Strain; 50 mm/min
Tensile Modulus 3.30 GPa1 mm/min
Charpy Impact Unnotched 2.00 J/cm²
Charpy Impact, Notched 0.200 J/cm²
Tensile Creep Modulus, 1 hour 2700 MPa
Tensile Creep Modulus, 1000 hours 1800 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
Dielectric Constant 3.2
@Frequency 1e+6 Hz
 3.7
@Frequency 100 Hz
Dielectric Strength 19.7 kV/mm
Dissipation Factor 0.040
@Frequency 1e+6 Hz
 0.050
@Frequency 100 Hz
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
Vicat Softening Point 107 °C50°C/hr; 50N
Flammability, UL94 HB
@Thickness 1.60 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Mfr. reports 'Transparent' but doesn't quantify.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Plexiglas® V825 Acrylic
Arkema Oroglas® V 825 HID Acrylic, UV, Heat Resistant
DuPont Mobility and Materials Delrin® 107 BK601 Acetal (POM) Homopolymer
DuPont Mobility and Materials Delrin® 107 NC010 Acetal (POM) Homopolymer
Mitsubishi Rayon Acrypet® VH-001 Heat Stabilized PMMA

PZARKG499 / 25757

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.