MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sandvik 19.9.LQ Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 19.9.LQ is particularly suited for welding in the nuclear industry. It is used for MIG, TIG, Plasma arc and submerged arc welding.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 160160TIG typical for non heat treated weld metal
Tensile Strength, Ultimate  360 MPa
@Temperature 350 °C
52200 psi
@Temperature 662 °F
SAW typical for non heat treated weld metal using flux 15W
 390 MPa
@Temperature 350 °C
56600 psi
@Temperature 662 °F
TIG typical for non heat treated weld metal
 540 MPa
@Temperature 20.0 °C
78300 psi
@Temperature 68.0 °F
SAW typical for non heat treated weld metal using flux 15W
 630 MPa
@Temperature 20.0 °C
91400 psi
@Temperature 68.0 °F
TIG typical for non heat treated weld metal
Tensile Strength, Yield  250 MPa
@Strain 0.2 %,
Temperature 350 °C
36300 psi
@Strain 0.2 %,
Temperature 662 °F
SAW typical for non heat treated weld metal using flux 15W
 270 MPa
@Strain 0.2 %,
Temperature 350 °C
39200 psi
@Strain 0.2 %,
Temperature 662 °F
TIG typical for non heat treated weld metal
 350 MPa
@Strain 0.2 %,
Temperature 20.0 °C
50800 psi
@Strain 0.2 %,
Temperature 68.0 °F
SAW typical for non heat treated weld metal using flux 15W
 420 MPa
@Strain 0.2 %,
Temperature 20.0 °C
60900 psi
@Strain 0.2 %,
Temperature 68.0 °F
TIG typical for non heat treated weld metal
Elongation at Break  33 %
@Temperature 350 °C
33 %
@Temperature 662 °F
SAW typical for non heat treated weld metal using flux 15W
 33 %
@Temperature 350 °C
33 %
@Temperature 662 °F
TIG typical for non heat treated weld metal
 38 %
@Temperature 20.0 °C
38 %
@Temperature 68.0 °F
TIG typical for non heat treated weld metal
 40 %
@Temperature 20.0 °C
40 %
@Temperature 68.0 °F
SAW typical for non heat treated weld metal using flux 15W
Reduction of Area 40 %40 %SAW typical for non heat treated weld metal using flux 15W
 60 %60 %TIG typical for non heat treated weld metal
Charpy Impact 140 J103 ft-lbTIG typical for non heat treated weld metal
 885 J653 ft-lbSAW typical for non heat treated weld metal using flux 15W
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %MIG
 0.020 %0.020 %SAW
 <= 0.025 %<= 0.025 %Aim
Chromium, Cr 19.5 %19.5 %Aim
 19.5 %19.5 %MIG
 19.5 %19.5 %SAW
Cobalt, Co 0.040 %0.040 %MIG
 0.040 %0.040 %SAW
 <= 0.050 %<= 0.050 %AIM
Copper, Cu 0.060 %0.060 %MIG
 0.070 %0.070 %SAW
 <= 0.10 %<= 0.10 %AIM
Manganese, Mn 1.4 %1.4 %SAW
 1.7 %1.7 %MIG
 1.8 %1.8 %Aim
Nickel, Ni 10 %10 %Aim
 10 %10 %MIG
 10 %10 %SAW
Nitrogen, N 0.050 %0.050 %MIG
 0.050 %0.050 %SAW
 <= 0.060 %<= 0.060 %Aim
Phosphorus, P 0.020 %0.020 %MIG
 0.025 %0.025 %SAW
 <= 0.025 %<= 0.025 %Aim
Silicon, Si 0.30 %0.30 %MIG
 0.40 %0.40 %Aim
 0.60 %0.60 %SAW
Sulfur, S 0.011 %0.011 %MIG
 0.012 %0.012 %SAW
 <= 0.015 %<= 0.015 %Aim

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Gall-Tough PLUS™ Stainless, Annealed at 1150°C

NSANDV5096 / 199660

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.